飽和麵幹(gān)試樣(yàng)的製(zhì)備(bèi),是將樣品在(zài)潮濕狀(zhuàng)態下用(yòng)四分(fēn)法縮(suō)分至(zhì)約1000G,拌匀後(hòu)分(fēn)成兩(liǎng)份,分別(bié)裝於淺(qiǎn)盤或其它合(hé)適(shì)的容(róng)器中,注(zhù)入清水,使水麵(miàn)高出(chū)試(shì)樣(yàng)表麵(miàn)20MM左右(水溫控製(zhì)在20±5℃)。用玻(bō)璃棒(bàng)連(lián)續攪拌5MIN,以(yǐ)排除(chú)氣泡。靜(jìng)置(zhì)24H以(yǐ)後(hòu),細心地(dì)倒(dǎo)去(qù)試(shì)樣上的水,並用吸管吸(xī)去餘水。再將試樣(yàng)在盤中(zhōng)攤(tān)開,用手提吹緩緩吹(chuī)入暖風(fēng),並不斷翻拌試樣,使砂表麵的(dí)水(shuǐ)分在各部位均(jūn)匀蒸(zhēng)發。然(rán)後(hòu)將試樣(yàng)鬆散(sàn)地一次(cì)裝(zhuāng)滿(mǎn)飽和(hé)麵幹試模中,搗(dǎo)25次(cì),搗(dǎo)棒距試樣表麵不(bù)超(chāo)過10MM,任(rèn)其自(zì)由(yóu)落(là)下,搗(dǎo)完後,留(liú)下的(dí)不(bù)用再(zài)裝滿,從垂直方(fāng)向(xiàng)徐徐(xú)提(tí)起試模。如試(shì)模呈(A)形(xíng)狀時,則說(shuō)明砂中尚(shàng)含有表麵水,應繼(jì)續按上述方法用暖(nuǎn)風幹燥,並按上述(shù)方法進行試(shì)驗,直至試模(mó)提起(qǐ)後試樣(yàng)呈(B)的(dí)形(xíng)狀(zhuàng)為止。如(rú)試(shì)模提(tí)起後,試(shì)樣呈(chéng)(C)的形狀,則說明試樣已幹燥過分,此時(shí)應將試樣(yàng)灑(sǎ)水(shuǐ)約55ML,充(chōng)分拌匀(yún),並(bìng)靜(jìng)置於加(jiā)蓋(gài)容器(qì)中30MIN後,再(zài)按上(shàng)述(shù)方(fāng)法(fǎ)進(jìn)行(háng)試驗(yàn),直(zhí)至試(shì)樣達(dá)到如(B)的形(xíng)狀(zhuàng)為止。河北精(jīng)威(wēi)試驗(yàn)儀器(qì)有限公(gōng)司提供(gōng)參(cān)數(shù)
備案(àn)號: 技(jì)術(shù)支(zhī)持(chí):